Link to full record for micrograph 173 Micrograph 173 : Bone china, showing the glaze on the surface (with sensitive tint plate)
System: Bone china, Composition: China clay 25, stone 30, bone 45 (wt% typical)
Transmitted polarised light microscopy, with sensitive tint plate
250 μm
Link to full record for micrograph 174 Micrograph 174 : Bone china (with sensitive tint plate)
System: Bone china, Composition: China clay 25, stone 30, bone 45 (wt% typical)
Transmitted polarised light microscopy, with sensitive tint plate
250 μm
Link to full record for micrograph 175 Micrograph 175 : Concrete from a commercial paving slab
System: Concrete, Composition: Aggregate, cement, water
Reflected light microscopy
100 μm
Link to full record for micrograph 176 Micrograph 176 : Concrete from a commercial paving slab
System: Concrete, Composition: Aggregate, cement, water
Reflected light microscopy
250 μm
Link to full record for micrograph 177 Micrograph 177 : Terracotta pottery
System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay.
Reflected light microscopy
200 μm
Link to full record for micrograph 178 Micrograph 178 : Terracotta pottery, showing the glaze on the surface
System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay.
Reflected light microscopy
100 μm
Link to full record for micrograph 179 Micrograph 179 : Terracotta pottery, showing the glaze on the surface
System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay.
Reflected light microscopy
250 μm
Link to full record for micrograph 180 Micrograph 180 : Oven-to-tableware showing the glaze on the surface, using a sensitive tint plate
System: Miscellaneous, Composition: Not specified
Transmitted polarised light microscopy, with sensitive tint plate
200 μm
Link to full record for micrograph 181 Micrograph 181 : Oven-to-tableware
System: Miscellaneous, Composition: Not specified
Transmitted polarised light microscopy, with sensitive tint plate
100 μm
Link to full record for micrograph 182 Micrograph 182 : Oven-to-tableware
System: Miscellaneous, Composition: Not specified
Transmitted polarised light microscopy
100 μm