Link to full record for micrograph 561 Micrograph 561 : Ordered film of carbon nanotubes
System: Carbon nanotube, Composition: Not specified
Field emission gun scanning electron microscopy (FEGSEM)
400 nm
Link to full record for micrograph 562 Micrograph 562 : Multi-walled carbon nanotube
System: Carbon nanotube, Composition: Not specified
Transmission electron microscopy (TEM)
3.2 nm
Link to full record for micrograph 563 Micrograph 563 : Carbon nanotubes
System: Carbon nanotube, Composition: Low concentration (<0.3 vol%) suspension in water
Field emission gun scanning electron microscopy (FEGSEM)
99 nm
Link to full record for micrograph 564 Micrograph 564 : Aligned array of nanotubes
System: Carbon nanotube, Composition: Not specified
Scanning electron microscopy (SEM)
25 μm
Link to full record for micrograph 565 Micrograph 565 : Vapour-grown carbon nanotubes
System: Carbon nanotube, Composition: Not specified
Scanning electron microscopy (SEM)
5 μm
Link to full record for micrograph 594 Micrograph 594 : Carbon string
System: C, Composition: Not specified
Scanning electron microscopy (SEM)
400 μm
Link to full record for micrograph 628 Micrograph 628 : Sintered salt (NaCl)
System: Na-Cl, Composition: Not specified
Scanning electron microscopy (SEM)
140 μm
Link to full record for micrograph 650 Micrograph 650 : Small ceramic pot showing centimetre scale crystals within the glaze
System: Soda-lime-silica glaze, Composition: Soda-lime-silica glaze containing zinc oxide 25, cobalt oxide 0.5 (wt%)
Photography (no microscope)
20 mm
Link to full record for micrograph 655 Micrograph 655 : Small ceramic pot showing centimetre scale crystals within the glaze
System: Soda-lime-silica glaze, Composition: Soda-lime-silica glaze containing zinc oxide 25, cobalt oxide 0.5 (wt%)
Photography (no microscope)
5 mm
Link to full record for micrograph 663 Micrograph 663 : Barium titanate ceramic
System: BaTiO3, Composition: Not specified
Reflected light microscopy
No length bar

Showing 61 - 70 of 92 micrographs Page 1 .. 4 5 6 7 8 9 10 | Previous | Next

Help is available on browsing.

Alternatively, search the Library (from top right on any page), or use advanced search.