Link to full record for micrograph 180 Micrograph 180 : Oven-to-tableware showing the glaze on the surface, using a sensitive tint plate
System: Miscellaneous, Composition: Not specified
Transmitted polarised light microscopy, with sensitive tint plate
200 μm
Link to full record for micrograph 181 Micrograph 181 : Oven-to-tableware
System: Miscellaneous, Composition: Not specified
Transmitted polarised light microscopy, with sensitive tint plate
100 μm
Link to full record for micrograph 182 Micrograph 182 : Oven-to-tableware
System: Miscellaneous, Composition: Not specified
Transmitted polarised light microscopy
100 μm
Link to full record for micrograph 183 Micrograph 183 : Oven-to-tableware
System: Miscellaneous, Composition: Not specified
Transmitted polarised light microscopy
250 μm
Link to full record for micrograph 184 Micrograph 184 : Oven-to-tableware
System: Miscellaneous, Composition: Not specified
Transmitted polarised light microscopy
250 μm