Categories > Ceramic > Miscellaneous > Transmitted polarised light microscopy, with sensitive tint plate > Keyword: ceramic

2 micrographs available, ordered by micrograph number.


Link to full record for micrograph 180 Micrograph 180 : Oven-to-tableware showing the glaze on the surface, using a sensitive tint plate
System: Miscellaneous, Composition: Not specified
Transmitted polarised light microscopy, with sensitive tint plate
200 μm
Link to full record for micrograph 181 Micrograph 181 : Oven-to-tableware
System: Miscellaneous, Composition: Not specified
Transmitted polarised light microscopy, with sensitive tint plate
100 μm