Categories > Ceramic > Triaxial (i.e. clay/flux/filler) porcelain

1 composition available. The number of micrographs available is given in [brackets].


Ball clay 30 , china clay 10, potash feldspar 20, silica sand 20, calcined alumina 20 (wt%) [1]