Browse the Library
Categories > Ceramic > MgO-C > Reflected light microscopy > Keyword: magnesia
2 micrographs available, ordered by micrograph number.
Micrograph
193
:
MgO-C Refractory Brick System: MgO-C, Composition: MgO 50-90, C 8-37 (wt%), remainder Al, Si metal addition Reflected light microscopy 200 μm |
|
Micrograph
194
:
MgO-C Refractory Brick System: MgO-C, Composition: MgO 50-90, C 8-37 (wt%), remainder Al, Si metal addition Reflected light microscopy 200 μm |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.