Browse the Library
Categories > Ceramic > ZrO2-Y2O3 > ZrO2 92.5, Y2O3 7.5 (wt%) > Field emission gun scanning electron microscopy (FEGSEM)
3 keywords available. The number of micrographs available is given in [brackets].
- partially stabilized zirconia (PSZ) [1]
- Show relevant: micrographs
- physical vapor deposition (PVD) [1]
- Show relevant: micrographs
- zirconia [1]
- Show relevant: micrographs
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.