Categories > Ceramic > Magnesia chromite > Keyword: clinker

4 micrographs available, ordered by micrograph number.


Link to full record for micrograph 675 Micrograph 675 : Magnesia-Chromite Clinker
System: Magnesia chromite, Composition: Magnesia 85, chromite 15 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 676 Micrograph 676 : Magnesia-Chromite Clinker
System: Magnesia chromite, Composition: Magnesia 85, chromite 15 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 677 Micrograph 677 : Magnesia-Chromite Clinker
System: Magnesia chromite, Composition: Magnesia 85, chromite 15 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 678 Micrograph 678 : Magnesia-Chromite Clinker
System: Magnesia chromite, Composition: Magnesia 85, chromite 15 (wt%)
Reflected light microscopy
50 μm