Categories > Ceramic > Hydroxyapatite (Ca10(PO4)6(OH)2) > Scanning electron microscopy (SEM)

1 micrograph available, ordered by micrograph number.


Link to full record for micrograph 117 Micrograph 117 : Sintered disc of Hydroxyapatite (Ca10(PO4)6(OH)2), a calcium phosphate ceramic with similar composition to natural bone mineral
System: Hydroxyapatite (Ca10(PO4)6(OH)2), Composition: Not specified
Scanning electron microscopy (SEM)
18 μm