Categories > Ceramic > ZnO > ZnO containing small amounts of oxides such as Sb2O3 and Bi2O3 > Keyword: zinc

2 micrographs available, ordered by micrograph number.


Link to full record for micrograph 170 Micrograph 170 : ZnO varistor
System: ZnO, Composition: ZnO containing small amounts of oxides such as Sb2O3 and Bi2O3
Transmitted polarised light microscopy, with sensitive tint plate
100 μm
Link to full record for micrograph 171 Micrograph 171 : ZnO varistor
System: ZnO, Composition: ZnO containing small amounts of oxides such as Sb2O3 and Bi2O3
Transmitted polarised light microscopy, with sensitive tint plate
250 μm