Categories > Ceramic > Reflected light microscopy > Keyword: barium titanate

3 micrographs available, ordered by micrograph number.


Link to full record for micrograph 153 Micrograph 153 : Barium Titanate Ag/Pd Multilayer Capacitor
System: BaTiO3 Ag/Pd, Composition: BaTiO3
Reflected light microscopy
300 μm
Link to full record for micrograph 663 Micrograph 663 : Barium titanate ceramic
System: BaTiO3, Composition: Not specified
Reflected light microscopy
No length bar
Link to full record for micrograph 664 Micrograph 664 : Barium titanate ceramic
System: BaTiO3, Composition: Not specified
Reflected light microscopy
No length bar