Browse the Library
Categories > Ceramic > Reflected light microscopy > Keyword: ceramic
37 micrographs available, ordered by micrograph number.
Showing 11 - 20 of 37 micrographs | Page 1 2 3 4 | Previous | Next |
Micrograph
175
:
Concrete from a commercial paving slab System: Concrete, Composition: Aggregate, cement, water Reflected light microscopy 100 μm |
|
Micrograph
176
:
Concrete from a commercial paving slab System: Concrete, Composition: Aggregate, cement, water Reflected light microscopy 250 μm |
|
Micrograph
177
:
Terracotta pottery System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay. Reflected light microscopy 200 μm |
|
Micrograph
178
:
Terracotta pottery, showing the glaze on the surface System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay. Reflected light microscopy 100 μm |
|
Micrograph
179
:
Terracotta pottery, showing the glaze on the surface System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay. Reflected light microscopy 250 μm |
|
Micrograph
185
:
Silicon Nitride-bonded Silicon Carbide System: Silicon nitride-bonded silicon carbide, Composition: Particles of SiC in a reaction-bonded Si3N4 matrix Reflected light microscopy 250 μm |
|
Micrograph
186
:
Silicon Carbide from within a Silicon Nitride-bonded Silicon Carbide sample System: Silicon nitride-bonded silicon carbide, Composition: Particles of SiC in a reaction-bonded Si3N4 matrix Reflected light microscopy 25 μm |
|
Micrograph
187
:
Part of a Denby pottery mug, showing the glaze on the surface System: Al2O3-SiO2, Composition: Mostly clay (which consists of alumina and silica) Reflected light microscopy 200 μm |
|
Micrograph
188
:
Part of a Denby pottery mug System: Al2O3-SiO2, Composition: Mostly clay (which consists of alumina and silica) Reflected light microscopy 200 μm |
|
Micrograph
193
:
MgO-C Refractory Brick System: MgO-C, Composition: MgO 50-90, C 8-37 (wt%), remainder Al, Si metal addition Reflected light microscopy 200 μm |