Categories > Ceramic > Reflected light microscopy > Keyword: iron

3 micrographs available, ordered by micrograph number.


Link to full record for micrograph 148 Micrograph 148 : Magnesia-chrome refractory brick
System: MgO-Cr2O3, Composition: MgO 70, Cr2O3 19, Al2O3 4, Fe2O3 4, CaO 1, SiO2 1 (wt%)
Reflected light microscopy
1 mm
Link to full record for micrograph 149 Micrograph 149 : Magnesia-chrome refractory brick
System: MgO-Cr2O3, Composition: MgO 70, Cr2O3 19, Al2O3 4, Fe2O3 4, CaO 1, SiO2 1 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 152 Micrograph 152 : Barium Hexaferrite
System: BaO-Fe2O3, Composition: BaO . 6Fe2O3
Reflected light microscopy
100 μm