Plasma sprayed (PS) partially stabilised zirconia (PSZ) showing splat morphology System: ZrO2-Yb2O3, Composition: ZrO2 84, Yb2O3 16 (wt%) Field emission gun scanning electron microscopy (FEGSEM) 2 μm |
|
Micrograph
848
:
Physical vapour deposited (PVD) partially stabilized zirconia (PSZ) showing columnar structure System: ZrO2-Y2O3, Composition: ZrO2 92.5, Y2O3 7.5 (wt%) Field emission gun scanning electron microscopy (FEGSEM) 1 μm |