Link to full record for micrograph 561 Micrograph 561 : Ordered film of carbon nanotubes
System: Carbon nanotube, Composition: Not specified
Field emission gun scanning electron microscopy (FEGSEM)
400 nm
Link to full record for micrograph 563 Micrograph 563 : Carbon nanotubes
System: Carbon nanotube, Composition: Low concentration (<0.3 vol%) suspension in water
Field emission gun scanning electron microscopy (FEGSEM)
99 nm
Link to full record for micrograph 847 Micrograph 847 : Plasma sprayed (PS) partially stabilised zirconia (PSZ) showing splat morphology
System: ZrO2-Yb2O3, Composition: ZrO2 84, Yb2O3 16 (wt%)
Field emission gun scanning electron microscopy (FEGSEM)
2 μm
Link to full record for micrograph 848 Micrograph 848 : Physical vapour deposited (PVD) partially stabilized zirconia (PSZ) showing columnar structure
System: ZrO2-Y2O3, Composition: ZrO2 92.5, Y2O3 7.5 (wt%)
Field emission gun scanning electron microscopy (FEGSEM)
1 μm