Categories > Composite > Al, Mg 2.5 (wt%), with Al2O3 (10 vol%) > Reflected light microscopy, polarised > Keyword: alumina
1 micrograph available, ordered by micrograph number.
![]() |
Micrograph
602
:
Section of a metal matrix composite (MMC) System: Al-Mg, Composition: Al, Mg 2.5 (wt%), with Al2O3 (10 vol%) Reflected light microscopy, polarised 80 μm |