Categories > Composite > Al, Mg 2.5 (wt%), with Al2O3 (10 vol%) > Reflected light microscopy, polarised > Keyword: infiltration

1 micrograph available, ordered by micrograph number.


Link to full record for micrograph 602 Micrograph 602 : Section of a metal matrix composite (MMC)
System: Al-Mg, Composition: Al, Mg 2.5 (wt%), with Al2O3 (10 vol%)
Reflected light microscopy, polarised
80 μm