DoITPoMS Micrograph Library Browse the Library

Browse the Library

Categories > Composite > Keyword: ceramic

12 micrographs available, ordered by micrograph number.


Showing 1 - 10 of 12 micrographs Page 1 2 | Previous | Next

Link to full record for micrograph 151 Micrograph 151 : Alumina-graphite brick
System: Al2O3-C-Si, Composition: Al2O3, C up to 30 (wt%), Si few%
Reflected light microscopy
400 μm
Link to full record for micrograph 175 Micrograph 175 : Concrete from a commercial paving slab
System: Concrete, Composition: Aggregate, cement, water
Reflected light microscopy
100 μm
Link to full record for micrograph 176 Micrograph 176 : Concrete from a commercial paving slab
System: Concrete, Composition: Aggregate, cement, water
Reflected light microscopy
250 μm
Link to full record for micrograph 193 Micrograph 193 : MgO-C Refractory Brick
System: MgO-C, Composition: MgO 50-90, C 8-37 (wt%), remainder Al, Si metal addition
Reflected light microscopy
200 μm
Link to full record for micrograph 194 Micrograph 194 : MgO-C Refractory Brick
System: MgO-C, Composition: MgO 50-90, C 8-37 (wt%), remainder Al, Si metal addition
Reflected light microscopy
200 μm
Link to full record for micrograph 195 Micrograph 195 : Zirconia Toughened Alumina (ZTA)
System: ZrO2-Al2O3, Composition: ZrO2 5-30, Al2O3 70-95 (wt%)
Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode
10 μm
Link to full record for micrograph 546 Micrograph 546 : Delamination cracks seen in h-BN particles subjected to compressive stress in the (0001) planes (within a silicon nitride particulate-reinforced silicon carbide composite)
System: Si3N4-SiC composite, Composition: Not specified
High resolution electron microscopy (HREM)
10 nm
Link to full record for micrograph 547 Micrograph 547 : h-BN inclusion (precipitate) in a b-Si3N4 grain (within a silicon nitride particulate-reinforced silicon carbide composite)
System: Si3N4-SiC composite, Composition: Not specified
High resolution electron microscopy (HREM)
20 nm
Link to full record for micrograph 549 Micrograph 549 : Misoriented interphase boundary between h-BN (precipitate) and SiC grains (within a silicon nitride particulate-reinforced silicon carbide composite)
System: Si3N4-SiC composite, Composition: Not specified
High resolution electron microscopy (HREM)
1.2 nm
Link to full record for micrograph 551 Micrograph 551 : A regularly stepped interface boundary between h-BN (precipitate) and Si3N4 grains (within a silicon nitride particulate-reinforced silicon carbide composite)
System: Si3N4-SiC composite, Composition: Not specified
High resolution electron microscopy (HREM)
10 nm

Showing 1 - 10 of 12 micrographs Page 1 2 | Previous | Next

Help is available on browsing.

Alternatively, search the Library (from top right on any page), or use advanced search.