2 micrographs available, ordered by micrograph number.
Micrograph
131
:
Unidirectional T800 carbon fibres in an MTM49 epoxy matrix. System: CCcomposite, Composition: Not specified Reflected light microscopy 250 μm |
|
Micrograph
132
:
Woven T800 carbon fibres in an MTM49 epoxy matrix. System: CCcomposite, Composition: Not specified Reflected light microscopy 200 μm |