Browse the Library
Categories > Composite > Barrikade > Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode > Keyword: filler
1 micrograph available, ordered by micrograph number.
Micrograph
624
:
Inter-particle bond in the fire-resistant composite Barrikade (R) System: Barrikade, Composition: Expanded vermiculite, cured in ZnO and mixed with binder Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 100 μm |
Help is available on browsing.