Categories > Composite > Scanning electron microscopy (SEM)

11 micrographs available, ordered by micrograph number.


Showing 1 - 10 of 11 micrographs Page 1 2 | Previous | Next

Link to full record for micrograph 579 Micrograph 579 : SEM image of open cell polyurethane foam
System: Polyurethane (PU), Composition: Not specified
Scanning electron microscopy (SEM)
800 μm
Link to full record for micrograph 580 Micrograph 580 : High magnification SEM image of open cell polyurethane foam
System: Polyurethane (PU), Composition: Not specified
Scanning electron microscopy (SEM)
160 μm
Link to full record for micrograph 582 Micrograph 582 : Low magnification SEM image of open cell polyurethane foam
System: Polyurethane (PU), Composition: Not specified
Scanning electron microscopy (SEM)
4 mm
Link to full record for micrograph 616 Micrograph 616 : Cavity formation in a tensile loaded alumina particulate composite
System: Al, Composition: Commercial purity (99.5%) + 15 micron angular alumina particles
Scanning electron microscopy (SEM)
80 μm
Link to full record for micrograph 618 Micrograph 618 : Fracture surface of a carbon fibre composite
System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
600 μm
Link to full record for micrograph 619 Micrograph 619 : Tensile failure surface of a carbon fibre composite
System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
100 μm
Link to full record for micrograph 620 Micrograph 620 : Kevlar fibre composite fracture surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
600 μm
Link to full record for micrograph 621 Micrograph 621 : Kevlar fibre composite shear surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
100 μm
Link to full record for micrograph 622 Micrograph 622 : Kevlar fibre composite shear surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
100 μm
Link to full record for micrograph 626 Micrograph 626 : Glass fibre reinforced thermoplastic matrix composite
System: Glass fibre composite, Composition: Polypropylene matrix with glass fibre
Scanning electron microscopy (SEM)
60 μm