Categories > Polymer > Not specified (Carbon nanotube) > Field emission gun scanning electron microscopy (FEGSEM) > Keyword: film

1 micrograph available, ordered by micrograph number.


Link to full record for micrograph 561 Micrograph 561 : Ordered film of carbon nanotubes
System: Carbon nanotube, Composition: Not specified
Field emission gun scanning electron microscopy (FEGSEM)
400 nm