Link to full record for micrograph 620 Micrograph 620 : Kevlar fibre composite fracture surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
600 μm
Link to full record for micrograph 621 Micrograph 621 : Kevlar fibre composite shear surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
100 μm
Link to full record for micrograph 622 Micrograph 622 : Kevlar fibre composite shear surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
100 μm
Link to full record for micrograph 640 Micrograph 640 : Fracture surface in a liquid crystalline polymer, oriented by a magnetic field
System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14401
Scanning electron microscopy (SEM)
4 μm
Link to full record for micrograph 641 Micrograph 641 : Fracture surface in a liquid crystalline polymer
System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14401
Scanning electron microscopy (SEM)
12 μm
Link to full record for micrograph 642 Micrograph 642 : Fracture surface in a liquid crystalline polymer
System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14402
Scanning electron microscopy (SEM)
12 μm