Browse the Library
Categories > Polymer > Keyword: polymer
69 micrographs available, ordered by micrograph number.
Showing 31 - 40 of 69 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |
Micrograph
582
:
Low magnification SEM image of open cell polyurethane foam System: Polyurethane (PU), Composition: Not specified Scanning electron microscopy (SEM) 4 mm |
|
Micrograph
583
:
SEM image of Velcro (TM) System: Nylon, Composition: Not specified Scanning electron microscopy (SEM) 400 μm |
|
Micrograph
584
:
External surface of blow-moulded HDPE System: High density polyethylene (HDPE), Composition: Not specified Scanning electron microscopy (SEM) 400 μm |
|
Micrograph
585
:
Internal surface of blow-moulded HDPE System: High density polyethylene (HDPE), Composition: Not specified Scanning electron microscopy (SEM) 6 μm |
|
Micrograph
586
:
Fracture surface in polystyrene System: Polystyrene (PS), Composition: Not specified Scanning electron microscopy (SEM) 160 μm |
|
Micrograph
587
:
Parabolic beach marks on a polystyrene fracture surface System: Polystyrene (PS), Composition: Not specified Scanning electron microscopy (SEM) 80 μm |
|
Micrograph
588
:
Beach marks on a polystyrene fracture surface System: Polystyrene (PS), Composition: Not specified Scanning electron microscopy (SEM) 50 μm |
|
Micrograph
589
:
Remnants of crazes on a polystyrene fracture surface System: Polystyrene (PS), Composition: Not specified Scanning electron microscopy (SEM) 8 μm |
|
Micrograph
590
:
Remnants of crazes on a polycarbonate fracture surface System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 10 μm |
|
Micrograph
591
:
Crazing near a fracture surface in polycarbonate System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 80 μm |
Showing 31 - 40 of 69 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.