Browse the Library
Categories > Polymer > Keyword: polymer
69 micrographs available, ordered by micrograph number.
Showing 61 - 69 of 69 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |
Micrograph
641
:
Fracture surface in a liquid crystalline polymer System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14401 Scanning electron microscopy (SEM) 12 μm |
|
Micrograph
642
:
Fracture surface in a liquid crystalline polymer System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14402 Scanning electron microscopy (SEM) 12 μm |
|
Micrograph
643
:
Aligned carbon nanotubes, coated with a conducting polymer System: Carbon nanotube, Composition: Coating of polypyrrole Scanning electron microscopy (SEM) 1 μm |
|
Micrograph
644
:
Carbon nanotubes, coated with a conducting polymer System: Carbon nanotube, Composition: Coating of polypyrrole Scanning electron microscopy (SEM) 100 nm |
|
Micrograph
645
:
An image of a single crystal alkane System: Alkane, Composition: C294H590 Transmission electron microscopy (TEM) 2.4 μm |
|
Micrograph
646
:
Spherulite growth imaged by atomic force microscopy (AFM) System: Polyhydroxybutyrate (PHB), Composition: Not specified Atomic force microscopy (AFM) 500 nm |
|
Micrograph
647
:
A spherulite imaged by atomic force microscopy (AFM) System: Polyhydroxybutyrate (PHB), Composition: Not specified Atomic force microscopy (AFM) 3 μm |
|
Micrograph
648
:
A spherulite imaged by atomic force microscopy (AFM) System: Polyhydroxybutyrate (PHB), Composition: Not specified Atomic force microscopy (AFM) 2 μm |
|
Micrograph
649
:
An image of an alkane crystal taken by AFM System: Alkane, Composition: C36H74 Atomic force microscopy (AFM) 30 μm |
Showing 61 - 69 of 69 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |
Help is available on browsing.