Categories > Polymer > High Impact Polystyrene (HIPS) > Keyword: tough

2 micrographs available, ordered by micrograph number.


Link to full record for micrograph 557 Micrograph 557 : High Impact Polystyrene (HIPS)
System: High Impact Polystyrene (HIPS), Composition: PS - 15%PB
Transmitted light microscopy
10 μm
Link to full record for micrograph 558 Micrograph 558 : High Impact Polystyrene (HIPS)
System: High Impact Polystyrene (HIPS), Composition: PS - 35%PB
Transmitted light microscopy
20 μm