Categories > Polymer > Polycarbonate (PC) > Scanning electron microscopy (SEM) > Keyword: shear bands

1 micrograph available, ordered by micrograph number.


Link to full record for micrograph 559 Micrograph 559 : Shear bands in stressed polycarbonate
System: Polycarbonate (PC), Composition: Not specified
Scanning electron microscopy (SEM)