Browse the Library
Categories > Polymer > Liquid crystalline polymer > Cross-polarised light microscopy > Keyword: polymer
6 micrographs available, ordered by micrograph number.
Micrograph
566
:
Inversion wall revealed by spontaneous band texture in a liquid crystalline polymer System: Liquid crystalline polymer, Composition: Rigid copolyester of hydroxybenzoate (HBA) and hydroxynapthoate (HNA) (1:1) Cross-polarised light microscopy 50 μm |
|
Micrograph
567
:
Wedge disclinations revealed by spontaneous band texture in a liquid crystalline polymer System: Liquid crystalline polymer, Composition: Rigid copolyester of hydroxybenzoate (HBA) and hydroxynapthoate (HNA) (1:1) Cross-polarised light microscopy 50 μm |
|
Micrograph
612
:
Nematic liquid crystalline polymer System: Liquid crystalline polymer, Composition: K24 (4-cyano-4'-8-alkylbiphenyl) Cross-polarised light microscopy 100 μm |
|
Micrograph
637
:
Disclinations in a smectic LCP, revealed by decoration System: Liquid crystalline polymer, Composition: Semi-flexible LCP, Cl-7 Cross-polarised light microscopy 10 μm |
|
Micrograph
638
:
Disclinations in a smectic LCP, revealed by decoration System: Liquid crystalline polymer, Composition: Semi-flexible LCP, Cl-8 Cross-polarised light microscopy 10 μm |
|
Micrograph
639
:
Twist-escaped loops in the liquid crystalline polymer MBBA System: Liquid crystalline polymer, Composition: MBBA Cross-polarised light microscopy 200 μm |
Help is available on browsing.