Categories > Polymer > Polypropylene (PP) > Cross-polarised light microscopy > Keyword: film
1 micrograph available, ordered by micrograph number.
Micrograph
572
:
Birefringence in a film of polypropylene System: Polypropylene (PP), Composition: Not specified Cross-polarised light microscopy 10 mm |