Browse the Library
Categories > Polymer > Polypropylene (PP) > Cross-polarised light microscopy > Keyword: sprue
1 micrograph available, ordered by micrograph number.
Micrograph
578
:
Sprue in a sample of polypropylene (PP) System: Polypropylene (PP), Composition: Not specified Cross-polarised light microscopy 10 mm |