Browse the Library
Categories > Polymer > High density polyethylene (HDPE) > Not specified > Keyword: surface
2 micrographs available, ordered by micrograph number.
Micrograph
584
:
External surface of blow-moulded HDPE System: High density polyethylene (HDPE), Composition: Not specified Scanning electron microscopy (SEM) 400 μm |
|
Micrograph
585
:
Internal surface of blow-moulded HDPE System: High density polyethylene (HDPE), Composition: Not specified Scanning electron microscopy (SEM) 6 μm |