Categories > Polymer > Polyhydroxybutyrate (PHB) > Atomic force microscopy (AFM)

3 micrographs available, ordered by micrograph number.


Link to full record for micrograph 646 Micrograph 646 : Spherulite growth imaged by atomic force microscopy (AFM)
System: Polyhydroxybutyrate (PHB), Composition: Not specified
Atomic force microscopy (AFM)
500 nm
Link to full record for micrograph 647 Micrograph 647 : A spherulite imaged by atomic force microscopy (AFM)
System: Polyhydroxybutyrate (PHB), Composition: Not specified
Atomic force microscopy (AFM)
3 μm
Link to full record for micrograph 648 Micrograph 648 : A spherulite imaged by atomic force microscopy (AFM)
System: Polyhydroxybutyrate (PHB), Composition: Not specified
Atomic force microscopy (AFM)
2 μm