Link to full record for micrograph 118 Micrograph 118 : Poly (lactic-co-glycolic acid) (PLGA) porous scaffold for tissue engineering. Average Pore Size 100-300 µm, porosity estimated at 65%
System: Poly (lactic-co-glycolic acid) (PLGA), Composition: Not specified
Scanning electron microscopy, environmental
400 μm