Categories > Polymer > Atomic force microscopy (AFM)

10 micrographs available, ordered by micrograph number.


Link to full record for micrograph 646 Micrograph 646 : Spherulite growth imaged by atomic force microscopy (AFM)
System: Polyhydroxybutyrate (PHB), Composition: Not specified
Atomic force microscopy (AFM)
500 nm
Link to full record for micrograph 647 Micrograph 647 : A spherulite imaged by atomic force microscopy (AFM)
System: Polyhydroxybutyrate (PHB), Composition: Not specified
Atomic force microscopy (AFM)
3 μm
Link to full record for micrograph 648 Micrograph 648 : A spherulite imaged by atomic force microscopy (AFM)
System: Polyhydroxybutyrate (PHB), Composition: Not specified
Atomic force microscopy (AFM)
2 μm
Link to full record for micrograph 649 Micrograph 649 : An image of an alkane crystal taken by AFM
System: Alkane, Composition: C36H74
Atomic force microscopy (AFM)
30 μm
Link to full record for micrograph 851 Micrograph 851 : Polystyrene
System: Polystyrene (PS), Composition: Polystyrene
Atomic force microscopy (AFM)
2 μm
Link to full record for micrograph 852 Micrograph 852 : Polystyrene
System: Polystyrene (PS), Composition: Polystyrene
Atomic force microscopy (AFM)
200 nm
Link to full record for micrograph 853 Micrograph 853 : Colloidal polymethyl methacrylate
System: Poly methyl methacrylate, Composition: Poly methyl methacrylate
Atomic force microscopy (AFM)
200 nm
Link to full record for micrograph 861 Micrograph 861 : Carbon
System: C, Composition: Carbon
Atomic force microscopy (AFM)
2 μm
Link to full record for micrograph 862 Micrograph 862 : Carbon
System: C, Composition: Carbon
Atomic force microscopy (AFM)
1 μm
Link to full record for micrograph 863 Micrograph 863 : Carbon
System: C, Composition: Carbon
Atomic force microscopy (AFM)
100 nm