Composition

7 micrographs for composition Fe, C 0.9 (wt%), ordered by micrograph number.

Link to full record for micrograph 27 Micrograph 27 : Fe, C 0.9 (wt%), martensite
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 28 Micrograph 28 : Fe, C 0.9 (wt%), martensite
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Scanning electron microscopy (SEM)
10 μm
Link to full record for micrograph 864 Micrograph 864 : Low Carbon Steel
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Atomic force microscopy (AFM)
2 μm
Link to full record for micrograph 865 Micrograph 865 : Low Carbon Steel
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Atomic force microscopy (AFM)
10 μm
Link to full record for micrograph 866 Micrograph 866 : Low Carbon Steel
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Atomic force microscopy (AFM)
5 μm
Link to full record for micrograph 867 Micrograph 867 : Low Carbon Steel
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Atomic force microscopy (AFM)
2 μm
Link to full record for micrograph 871 Micrograph 871 : Low Carbon Steel
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Atomic force microscopy (AFM)
30 μm