Composition

5 micrographs for composition Not specified (System: Polyhydroxybutyrate (PHB)), ordered by micrograph number.

Link to full record for micrograph 600 Micrograph 600 : Spherulite in poly-3-hydroxy butyrate (PHB)
System: Polyhydroxybutyrate (PHB), Composition: Not specified
Cross-polarised light microscopy
1 μm
Link to full record for micrograph 601 Micrograph 601 : Spherulites in in poly-3-hydroxy butyrate (PHB)
System: Polyhydroxybutyrate (PHB), Composition: Not specified
Cross-polarised light microscopy
240 nm
Link to full record for micrograph 646 Micrograph 646 : Spherulite growth imaged by atomic force microscopy (AFM)
System: Polyhydroxybutyrate (PHB), Composition: Not specified
Atomic force microscopy (AFM)
500 nm
Link to full record for micrograph 647 Micrograph 647 : A spherulite imaged by atomic force microscopy (AFM)
System: Polyhydroxybutyrate (PHB), Composition: Not specified
Atomic force microscopy (AFM)
3 μm
Link to full record for micrograph 648 Micrograph 648 : A spherulite imaged by atomic force microscopy (AFM)
System: Polyhydroxybutyrate (PHB), Composition: Not specified
Atomic force microscopy (AFM)
2 μm