7 micrographs for composition Commercial purity (99.5%), ordered by micrograph number.

Link to full record for micrograph 604 Micrograph 604 : Extruded aluminium
System: Al, Composition: Commercial purity (99.5%)
Reflected light microscopy, polarised
40 μm
Link to full record for micrograph 605 Micrograph 605 : Fracture surface formed by hot tearing (solidification cracking)
System: Al, Composition: Commercial purity (99.5%)
Scanning electron microscopy (SEM)
40 μm
Link to full record for micrograph 606 Micrograph 606 : Extruded Saffil-containing metal matrix composite
System: Al, Composition: Commercial purity (99.5%)
Reflected light microscopy, polarised
40 μm
Link to full record for micrograph 607 Micrograph 607 : Fibre fracture in a metal matrix composite
System: Al, Composition: Commercial purity (99.5%)
Scanning electron microscopy (SEM)
4 μm
Link to full record for micrograph 608 Micrograph 608 : Channelling contrast TEM image of subgrains of extruded aluminium
System: Al, Composition: Commercial purity (99.5%)
Transmission electron microscopy (TEM)
600 nm
Link to full record for micrograph 609 Micrograph 609 : The grain structure of extruded aluminium
System: Al, Composition: Commercial purity (99.5%)
Reflected light microscopy, polarised
40 μm
Link to full record for micrograph 615 Micrograph 615 : Cross-section of an aluminium casting
System: Al, Composition: Commercial purity (99.5%)
Reflected light microscopy
10 mm