Composition
1 micrograph for composition Not specified (System: Na-Cl), ordered by micrograph number.
Micrograph
628
:
Sintered salt (NaCl) System: Na-Cl, Composition: Not specified Scanning electron microscopy (SEM) 140 μm |
Dissemination of IT for the Promotion of Materials Science (DoITPoMS)
1 micrograph for composition Not specified (System: Na-Cl), ordered by micrograph number.
Micrograph
628
:
Sintered salt (NaCl) System: Na-Cl, Composition: Not specified Scanning electron microscopy (SEM) 140 μm |