Contributor
1 micrograph contributed by Prof W Kurz, ordered by micrograph number.
Micrograph
617
:
Deeply etched Co-dendrites System: Co-Sm-Cu, Composition: Co 70, Sm 10, Cu 20 (at%) Scanning electron microscopy (SEM) 80 μm |
Dissemination of IT for the Promotion of Materials Science (DoITPoMS)
1 micrograph contributed by Prof W Kurz, ordered by micrograph number.
Micrograph
617
:
Deeply etched Co-dendrites System: Co-Sm-Cu, Composition: Co 70, Sm 10, Cu 20 (at%) Scanning electron microscopy (SEM) 80 μm |