148
:
Magnesia-chrome refractory brick System: MgO-Cr2O3, Composition: MgO 70, Cr2O3 19, Al2O3 4, Fe2O3 4, CaO 1, SiO2 1 (wt%) Reflected light microscopy 1 mm |