Link to full record for micrograph 150 Micrograph 150 : Alumina-zirconia-silica (AZS) refractory brick
System: Al2O3-ZrO2-SiO2, Composition: Al2O3 50, ZrO2 32, SiO2 15 (wt%), + trace alkalis
Reflected light microscopy
300 μm
Link to full record for micrograph 154 Micrograph 154 : Macor(TM) Machinable Glass Ceramic
System: MAS (MgO-Al2O3-SiO2), Composition: SiO2 47, B2O3 8, Al2O3 17, MgO 14, K2O 9, F 6 (wt%)
Reflected light microscopy
20 μm
Link to full record for micrograph 160 Micrograph 160 : Glass ceramic, heat treated at 750° C for 3 hours
System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified
Transmitted polarised light microscopy, with sensitive tint plate
100 μm
Link to full record for micrograph 161 Micrograph 161 : Glass ceramic, heat treated at 750°C for 3 hours
System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified
Transmitted polarised light microscopy
100 μm
Link to full record for micrograph 162 Micrograph 162 : Glass ceramic, heat treated at 840°C for 3 hours
System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified
Transmitted polarised light microscopy, with sensitive tint plate
100 μm
Link to full record for micrograph 163 Micrograph 163 : Glass ceramic, heat treated at 840°C for 3 hours
System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified
Transmitted polarised light microscopy
100 μm
Link to full record for micrograph 164 Micrograph 164 : Glass ceramic, heat treated at 900°C for 3 hours
System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified
Transmitted polarised light microscopy, with sensitive tint plate
100 μm
Link to full record for micrograph 165 Micrograph 165 : Glass ceramic, heat treated at 900°C for 3 hours
System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified
Transmitted polarised light microscopy
100 μm
Link to full record for micrograph 542 Micrograph 542 : Devitrified Glass: glass sample heated at 900°C for 17 hours.
System: SiO2, Composition: Mostly silica, SiO2
Transmitted polarised light microscopy, with sensitive tint plate
100 μm
Link to full record for micrograph 543 Micrograph 543 : Devitrified Glass: glass sample heated at 900°C for 17 hours
System: SiO2, Composition: Mostly silica, SiO2
Transmitted polarised light microscopy, with sensitive tint plate
250 μm