1 micrograph for keyword porcelain, ordered by micrograph number.


Link to full record for micrograph 190 Micrograph 190 : Aluminous Electrical Porcelain
System: Triaxial (i.e. clay/flux/filler) porcelain, Composition: Ball clay 30 , china clay 10, potash feldspar 20, silica sand 20, calcined alumina 20 (wt%)
Scanning electron microscopy (SEM)
10 μm