Link to full record for micrograph 62 Micrograph 62 : Fe, C 3.6, Si 2.1 (wt%), hypereutectic grey cast iron
System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 63 Micrograph 63 : Fe, C 3.6, Si 2.1 (wt%), hypereutectic grey cast iron
System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 64 Micrograph 64 : Fe, C 3.6, Si 2.1, Mg 0.07 (wt%), spheroidal graphite
System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1, Mg 0.07 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 65 Micrograph 65 : Fe, C 3.6, Si 2.1, Mg 0.07 (wt%), spheroidal graphite
System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1, Mg 0.07 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 70 Micrograph 70 : Silal
System: Fe-C-X, Composition: Fe, C 3.0, Si 6, Mn 0.7, P 0.3, S 0.1 (wt% typical) (Silal)
Reflected light microscopy
200 μm
Link to full record for micrograph 71 Micrograph 71 : Silal
System: Fe-C-X, Composition: Fe, C 3.0, Si 6, Mn 0.7, P 0.3, S 0.1 (wt% typical) (Silal)
Reflected light microscopy
80 μm
Link to full record for micrograph 151 Micrograph 151 : Alumina-graphite brick
System: Al2O3-C-Si, Composition: Al2O3, C up to 30 (wt%), Si few%
Reflected light microscopy
400 μm
Link to full record for micrograph 193 Micrograph 193 : MgO-C Refractory Brick
System: MgO-C, Composition: MgO 50-90, C 8-37 (wt%), remainder Al, Si metal addition
Reflected light microscopy
200 μm
Link to full record for micrograph 194 Micrograph 194 : MgO-C Refractory Brick
System: MgO-C, Composition: MgO 50-90, C 8-37 (wt%), remainder Al, Si metal addition
Reflected light microscopy
200 μm
Link to full record for micrograph 777 Micrograph 777 : Grey cast iron (flake graphite)
System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5 (wt%)
Reflected light microscopy