18 micrographs for keyword hypereutectoid, ordered by micrograph number.


Showing 1 - 10 of 18 micrographs Page 1 2 | Previous | Next

Link to full record for micrograph 21 Micrograph 21 : Fe, C 1.0 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 22 Micrograph 22 : Fe, C 1.0 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 23 Micrograph 23 : Fe, C 1.0 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Scanning electron microscopy (SEM)
50 μm
Link to full record for micrograph 24 Micrograph 24 : Fe, C 1.0 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Scanning electron microscopy (SEM)
10 μm
Link to full record for micrograph 25 Micrograph 25 : Fe, C 0.85 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 0.85 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 26 Micrograph 26 : Fe, C 0.85 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 0.85 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 243 Micrograph 243 : Fe, C 1.3 (wt%) steel, annealed at 1100°C
System: Fe-C-X, Composition: Fe, C 1.3 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 244 Micrograph 244 : Fe, C 1.3 (wt%) steel, annealed at 1100°C
System: Fe-C-X, Composition: Fe, C 1.3 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 245 Micrograph 245 : Fe, C 1.3 (wt%) steel, normalised at 1050°C
System: Fe-C-X, Composition: Fe, C 1.3 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 246 Micrograph 246 : Fe, C 1.3 (wt%) steel, normalised at 1050°C
System: Fe-C-X, Composition: Fe, C 1.3 (wt%)
Reflected light microscopy
200 μm

Showing 1 - 10 of 18 micrographs Page 1 2 | Previous | Next