Keyword
1 micrograph for keyword Gasar, ordered by micrograph number.
Micrograph
634
:
Solid-gas eutectic solidification (Gasar) aluminium foam System: Al, Composition: Not specified Photography (no microscope) 120 μm |
Dissemination of IT for the Promotion of Materials Science (DoITPoMS)
1 micrograph for keyword Gasar, ordered by micrograph number.
Micrograph
634
:
Solid-gas eutectic solidification (Gasar) aluminium foam System: Al, Composition: Not specified Photography (no microscope) 120 μm |