12 micrographs for keyword liquid crystalline polymer (LCP), ordered by micrograph number.


Showing 1 - 10 of 12 micrographs Page 1 2 | Previous | Next

Link to full record for micrograph 566 Micrograph 566 : Inversion wall revealed by spontaneous band texture in a liquid crystalline polymer
System: Liquid crystalline polymer, Composition: Rigid copolyester of hydroxybenzoate (HBA) and hydroxynapthoate (HNA) (1:1)
Cross-polarised light microscopy
50 μm
Link to full record for micrograph 567 Micrograph 567 : Wedge disclinations revealed by spontaneous band texture in a liquid crystalline polymer
System: Liquid crystalline polymer, Composition: Rigid copolyester of hydroxybenzoate (HBA) and hydroxynapthoate (HNA) (1:1)
Cross-polarised light microscopy
50 μm
Link to full record for micrograph 612 Micrograph 612 : Nematic liquid crystalline polymer
System: Liquid crystalline polymer, Composition: K24 (4-cyano-4'-8-alkylbiphenyl)
Cross-polarised light microscopy
100 μm
Link to full record for micrograph 620 Micrograph 620 : Kevlar fibre composite fracture surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
600 μm
Link to full record for micrograph 621 Micrograph 621 : Kevlar fibre composite shear surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
100 μm
Link to full record for micrograph 622 Micrograph 622 : Kevlar fibre composite shear surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
100 μm
Link to full record for micrograph 637 Micrograph 637 : Disclinations in a smectic LCP, revealed by decoration
System: Liquid crystalline polymer, Composition: Semi-flexible LCP, Cl-7
Cross-polarised light microscopy
10 μm
Link to full record for micrograph 638 Micrograph 638 : Disclinations in a smectic LCP, revealed by decoration
System: Liquid crystalline polymer, Composition: Semi-flexible LCP, Cl-8
Cross-polarised light microscopy
10 μm
Link to full record for micrograph 639 Micrograph 639 : Twist-escaped loops in the liquid crystalline polymer MBBA
System: Liquid crystalline polymer, Composition: MBBA
Cross-polarised light microscopy
200 μm
Link to full record for micrograph 640 Micrograph 640 : Fracture surface in a liquid crystalline polymer, oriented by a magnetic field
System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14401
Scanning electron microscopy (SEM)
4 μm