Dissemination of IT for the Promotion of Materials Science (DoITPoMS)

Keyword

2 micrographs for keyword polyethylene terephthalate (PET), ordered by micrograph number.


Link to full record for micrograph 568 Micrograph 568 : Strain induced birefringence in a thermoformed PET cup
System: Polyethylene terephthalate (PET), Composition: Not specified
Cross-polarised light microscopy
8 mm
Link to full record for micrograph 625 Micrograph 625 : Series of laser welds in amorphous PET
System: Polyethylene terephthalate (PET), Composition: Amorphous polyethylene terephthalate (APET)
Cross-polarised light microscopy
12 mm

List all keywords