Keyword
1 micrograph for keyword soldidification, ordered by micrograph number.
Micrograph
614
:
Rapid solidification in an atomised droplet System: Al-Mg, Composition: Al 90, Mg 10 (wt%) Transmission electron microscopy (TEM) 500 nm |