Dissemination of IT for the Promotion of Materials Science (DoITPoMS)

Keyword

7 micrographs for keyword texture, ordered by micrograph number.


Link to full record for micrograph 566 Micrograph 566 : Inversion wall revealed by spontaneous band texture in a liquid crystalline polymer
System: Liquid crystalline polymer, Composition: Rigid copolyester of hydroxybenzoate (HBA) and hydroxynapthoate (HNA) (1:1)
Cross-polarised light microscopy
50 μm
Link to full record for micrograph 567 Micrograph 567 : Wedge disclinations revealed by spontaneous band texture in a liquid crystalline polymer
System: Liquid crystalline polymer, Composition: Rigid copolyester of hydroxybenzoate (HBA) and hydroxynapthoate (HNA) (1:1)
Cross-polarised light microscopy
50 μm
Link to full record for micrograph 637 Micrograph 637 : Disclinations in a smectic LCP, revealed by decoration
System: Liquid crystalline polymer, Composition: Semi-flexible LCP, Cl-7
Cross-polarised light microscopy
10 μm
Link to full record for micrograph 638 Micrograph 638 : Disclinations in a smectic LCP, revealed by decoration
System: Liquid crystalline polymer, Composition: Semi-flexible LCP, Cl-8
Cross-polarised light microscopy
10 μm
Link to full record for micrograph 646 Micrograph 646 : Spherulite growth imaged by atomic force microscopy (AFM)
System: Polyhydroxybutyrate (PHB), Composition: Not specified
Atomic force microscopy (AFM)
500 nm
Link to full record for micrograph 647 Micrograph 647 : A spherulite imaged by atomic force microscopy (AFM)
System: Polyhydroxybutyrate (PHB), Composition: Not specified
Atomic force microscopy (AFM)
3 μm
Link to full record for micrograph 648 Micrograph 648 : A spherulite imaged by atomic force microscopy (AFM)
System: Polyhydroxybutyrate (PHB), Composition: Not specified
Atomic force microscopy (AFM)
2 μm

List all keywords