Keyword
1 micrograph for keyword urea formaldehyde, ordered by micrograph number.
Micrograph
595
:
Thermoset case of an electrical plug System: Urea formaldehyde, Composition: Not specified Reflected light microscopy 100 μm |
Dissemination of IT for the Promotion of Materials Science (DoITPoMS)
1 micrograph for keyword urea formaldehyde, ordered by micrograph number.
Micrograph
595
:
Thermoset case of an electrical plug System: Urea formaldehyde, Composition: Not specified Reflected light microscopy 100 μm |